UV15DC80Med USP Class VI approved one component UV and heat curable epoxy. Passes ISO 10993-5 cytotoxicity testing. Cures at temperatures as low as 80°C. Moderate viscosity. Minimal shrinkage upon cure. Capable of withstanding liquid sterilants, radiation, autoclaving. Serviceable from -60°F to +400°F. |
![]() |
UV15DC80ND UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. |
![]() |
UV15DC80TK UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator. |
![]() |
UV15FL Low viscosity epoxy system with enhanced toughness. Substantial temperature resistance, especially when post cured with heat. 100% reactive. Shore D hardnes >75. Tensile strength >5,000 psi. Optically clear, spin coatable. Serviceable from -80°F to +350°F. |
![]() |
UV15LV Low viscosity, high strength epoxy resin based formulation. Enhanced thermal stability. Cationic curing system. Excellent light transmission properties. Superb electrical insulation characteristics. Serviceable from -80°F to +300°F. |
![]() |
UV15TK Moderate viscosity single part UV curable epoxy. Cures quickly. Excellent dimensional stability. Enhanced temperature resistance. Cationic curing system. Optically clear. Volume resistivit >1014. Serviceable from -80°F to +400°F. |
![]() |
UV15X-2 For bonding, sealing, coating, encapsulation. Fast curing no mix compound. Excellent abrasion resistant. Viscosity 3,000-9,000 cps. Shore D hardnes >70. Impressive physical strength properties. Serviceable from -80°F to 300°F. |
![]() |
UV15X-2GT One part, UV curable epoxy with ultra fast curing. Good physical properties and chemical resistance. Used for glob top applications. Thixotropic paste viscosity. Excellent toughness. Withstands thermal cycling. Shore D hardness 65. Serviceable from -80°F to +250°F. |
![]() |
UV15X-5 Tough, abrasion resistant UV curing urethane acrylate type system. Non-yellowing capabilities. Resists thermal cycling and mechanical shocks. Elongatio >200%. Very fast curing. High viscosity. Serviceable from -80°F to +250°F. |
![]() |
UV15X-6Med-2 UV curing system with high flexibility that is biocompatible per USP Class VI testing. Medium viscosity. Superior abrasion resistance. Non-yellowing. Reliable thermal and electrical insulator. Serviceable from -80°F to +250°F. |