EP30F
Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Key Features
- Superb optical clarity
- Fast setting
- Low viscosity
- High bonding strength to a wide variety of substrates
Typical Properties
Viscosity
Part A: 300-700 cps, Part B: 2,000-4,000 cps
Cure Schedule
overnight at 75°F, followed by 1-2 hours at 150-200°F
Hardness
>75 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Constant
3.55
Dielectric Strength
440 volts/mil
Dissipation Factor
0.005
Linear Shrinkage
less than 0.003 in./in.
Refractive Index
1.57
Volume Resistivity
>10¹⁵ ohm-cm
Image
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863