Master Bond UV26 is a new one part UV curable system featuring an exceptionally high glass transition temperature (Tg) ranging from 160 to 170°C.
This NASA low outgassing certified compound also offers strong adhesion to a wide variety of substrates such as glass, surface treated metals and many plastics.
Master Bond EP41S-6 is a new two component epoxy system that meets UL 1203, which is defined by Underwriters Laboratories as the
“Standard for Explosion-Proof and Dust-Ignition-Proof Electrical Equipment for Use in Hazardous (Classified) Locations”.
Master Bond EP110F8-3 is a two part epoxy system ideal for sealing, encapsulating, potting, and casting applications.
“This toughened system provides very good flexibility and possesses a relatively high elongation of 120-150%”, says Rohit Ramnath, Senior Product Engineer.
Master Bond EP70CN is a two part, thermally stable epoxy adhesive formulated using a natural, renewable and sustainable ingredient.
This epoxy system forms high physical strength bonds and can be utilized for bonding, sealing, coating and potting.
Master Bond EP21ND-LP was created for structural bonding applications involving large surface areas.
It has an advantageously long working life of 2-4 hours at 75°F for a 100 gram mass.
Its smooth paste consistency makes it convenient to apply and use. Shore D hardness is 70-80 when mixed in a one to one mix ratio by weight or volume.
Master Bond EP30LTE-2 has been developed for joining dissimilar substrates exposed to thermally or mechanically induced stresses.
It can be used for sealing, coating and encapsulating, especially for small to medium sized castings where a very low coefficient of thermal expansion (CTE) is required.