MasterSil 801 One component, silicone paste resists up to 300°C (572°F). Elongation 250-350%. Extremely soft. Non-corrosive cure. Available in tube, jar and cartridge containers. |
|
MasterSil 803 Unique non-corrosive neutral curing oxime type silicone featuring enhanced high and low temperature serviceability from -180°F up to +500°F(260°C). Features high bond strength and superior electrical insulation properties. Paste viscosity. |
|
|
MasterSil 910Med Acetoxy type system. Bonding, sealing, coating compound. Pass USP Class VI testing and ISO cytotoxicity specifications. Tack free time 10-20 minutes at 75°F. Shore A hardness 20-30. Elongation 400-600%. Paste viscosity. Service temperature range -75°F to +400°F. |
|
MasterSil 912Med Single component silicone with a paste viscosity for bonding, sealing and coating medical devices. Non-corrosive, neutral cure compound complies with USP Class VI and ISO 10993-5 specifications. Resists many kinds of sterilization including gamma and other types of radiation, EtO and some types of liquid sterilants. |
|
MasterSil 913Med Acetoxy type system. Bonding, sealing, coating compound. Pass ISO cytotoxicity specifications. Tack free time 10-20 minutes at 75°F. Shore A hardness 20-30. Elongation 600-700%. Paste viscosity. Service temperature range -75°F to +400°F. |
|
MasterSil 920-LO RTV silicone for sealing, coating and small encapsulation. NASA low outgassing approved. Superb optical clarity. Good flow properties. Non-corrosive. Soft durometer facilitates usage with sensitive components. Excellent electrical insulator. Withstands thermal cycling. |
|
MasterSil 921-LO Passes NASA low outgassing test requirements. Spreads evenly and smoothly. Bonds well to many substrates. Wide service temperature range of -175°F to +500°F. Neutral curing, non-corrosive type system. |
|
MasterSil 922-LO Blended RTV silicone pastefor bonding, sealing, coating. Vibration and shock resistant. Withstands aggressive thermal cycling. NASA low outgassing approved. Serviceable from -175°F to 500°F. |
|
MasterSil 930 Acetoxy type fluorosilicone for bonding, sealing, coating. Enhanced resistance to fuels, oils, solvents, water, greases. Paste viscosity. Withstands thermal cycling. Serviceable up to +450°F. No mix system. |
|
MasterSil 970-LO Moderate viscosity, two component silicone adhesive, sealant, encapsulant. Passes NASA low outgassing test requirements. Vacuum compatible. Withstands rigorous thermal cycling and shock. White color. Good flow properties. Serviceable from -120°F to +400°F. |