MB250NT One Part Ethyl Cyanoacrylate System MB250NT

Low viscosity ethyl cyanoacrylate. Rapid curing at room temperature; usually sets up within 40 seconds. Passes ISO 10993-5 for cytotoxicity. Resistant to EtO and gamma sterilization. Serviceable from -60°F to +250°F.

MB295 Cyanoacrylate Adhesive MB295

Transparent adhesive. Shore A hardness 85. Bonds well to metals, plastics, glass, rubbers. Fast curing. Viscosity 1,300 to 1,700 cps.

MB297 One Part Ethyl Cyanoacrylate System MB297

Higher viscosity (2,200-2,400 cps) and a slightly longer open time than low viscosity counterparts. High strength, rapid curing ethyl cyanoacrylate system. No heating or mixing needed. Good resistance to cleaning agents. Serviceable from -60°F to +250°F.

One Part Cyanoacrylate MB297FL MB297FL

Flexibilized cyanoacrylate adhesive offers improved resistance to vibration.1,500-1,800 cps viscosity. Serviceable from -65°F to +185°F.

One Part Cyanoacrylate MB297FLNT MB297FLNT

Low viscosity ethyl cyanoacrylate. Rapid curing at room temperature; usually sets up within 40 seconds. Passes ISO 10993-5 for cytotoxicity. Resistant to EtO and gamma sterilization. Serviceable from -60°F to +250°F.

MB297Med One Part Ethyl Cyanoacrylate Compound MB297Med

Fast setting. Viscosity 2,000 - 2,400 cps. Biocompatible. Resists EtO and gamma sterilization. Passes USP Class VI testing. Bonds well to metals, plastics, rubbers, glass. Serviceable from -60°F to +250°F.

MB297Med-1 One Part Ethyl Cyanoacrylate Adhesive MB297Med-1

Moderate viscosity 1,000-1,100 cps. Rapid curing. Meets USP Class VI specifications. For disposable and reusable medical devices. Serviceable from -60°F to +250°F.

MB297Med-2 One Part Ethyl Cyanoacrylate Compound MB297Med-2

Fast setting. Low viscosity 100-110 cps. Meets USP Class VI specifications. For disposable and reusable medical devices. Serviceable from -60°F to +250°F.

MB297Med-3 Single Component Ethyl cyanoacrylate MB297Med-3

High bond strength. Rapid fixture time. Ultra low viscosity 10-20 cps. USP Class VI approved. For disposable and reusable medical devices. Serviceable from -60°F to +250°F.

MB306 One Part Ethyl Cyanoacrylate System MB306

Low viscosity methyl cyanoacrylate with superior bonding properties especially to metals. Contact pressure usually sufficient for fixturing. Viscosity 75-95 cps. Shore D hardness 70. Fast curing. Serviceable from -60°F to +250°F.