EP101HTX-3 Optically clear one component epoxy has outstanding electrical insulation properties. Viscosity 300-1,000 cps. Service temperature range from -60 to +500°F. Excellent thermal shock resistance. |
![]() |
EP112 Potting, encapsulation, coating, sealing, impregnation compound. Superior optical clarity and physical strength.Low dielectric constant and low dissipation factor. Stands up to 1,000 hours 85°C/85% RH. Long working life. Serviceable from -60°F to 450°F. |
![]() |
EP112LS Potting, encapsulation, sealing and impregnation compound. Low viscosity two component epoxy system. Heat curable. Long working life at room temperature. Superb optical clarity. Non-yellowing. Serviceable from -60°F to +450°F. High dielectric strength. |
![]() |
EP113 Two component nanosilica filled epoxy for potting, coating and sealing. Optically clear. Low shrinkage. Superior electrical insulation properties. Toughened system. Successfully tested for 1,000 hours 85°C/85% RH. Serviceable from -100°F to +450°F. |
![]() |
EP114 Two component nanosilica filled epoxy for potting, coating and sealing. Optically clear. Low shrinkage. Superior electrical insulation properties. Toughened system. Successfully tested for 1,000 hours 85°C/85% RH. Serviceable from -100°F to +450°F. |
![]() |
EP121CL Low viscosity epoxy with an extraordinary long open time. Superior dielectric strength. Impressive optical clarity. Excellent chemical resistance. Serviceable from -80°F to +500°F. |
![]() |
EP121CL-LO NASA low outgassing approved two component epoxy. Low viscosity system. High dielectric strength. Optically clear. Withstands 1,000 hours 85°C/85% RH. Shore D hardness 80-90. Serviceable from -80°F to +500°F. Long open time at room temperature. |
![]() |
EP21H Two component optically clear epoxy system. Special cross linking profile that allows for exceptional light transmission in the 250-365 nm spectra Long pot life. Low viscosity. Excellent physical strength properties. Serviceable from -60°F to +250°F. |
![]() |
EP21LSCL-2 Superb optical clarity. Non-yellowing properties. Two component low viscosity epoxy resin system. Long working life. Excellent electrical insulator. Used for large volume potting applications. Serviceable from -60°F to +250°F. |
![]() |
EP21NDCL Two component, room temperature curing non-flowing epoxy paste. Cures optically clear in thin sections. Superior physical strength profile. Non-critical one to one mix ratio by weight or volume. Service temperature range from -60°F to 250°F. Withstands 1,000 hours 85°C/85% RH. |