Two component, epoxy compound with a paste consistency, outstanding shear and peel strength for bonding, sealing and coating, featuring excellent adhesion to engineering plastics and metals, especially polycarbonates and acrylics
Two Component, Room Temperature Setting, Heat Resistant Epoxy System for Bonding, Sealing, Coating & Casting Specially Formulated for Indirect Food Applications.
UL94HB flame retardant, two component epoxy system. For encapsulating and coating that passes UL746A high amp arc ignition at 3.0 mm thickess with a PLC of 0. Convenient processing, 1:1 mix ratio by weight.
One component epoxy for bonding, sealing and small encapsulation applications, curing temperature 80°C. Thermally conductive, electrically insulating, high compressive strength..