187 products match
![]() |
EP42HT-2AO Thermally conductive, electrically insulative. Ideal for potting and encapsulation. Castable up to 3-4 inches. Excellent chemical resistance. Enhanced thermal cycling capabilities. Good flow. Serviceable from -100°F to +400°F. Impervious to intermittent exposures to steam. Shore D hardnes >80. |
![]() |
EP42HT-2AO-1 Black Good heat conduction. Serviceable from 4K to +400°F. Resists water, oils, fuels. Excellent dielectric properties. Enhanced dimensional stability. Castable up to 2-3 inches thick. Low shrinkage upon cure. Good flow. Meets NASA low outgassing standards. |
![]() |
EP42HT-3AO Thermally conductive, electrically insulative. Ideal for potting and encapsulation. Castable up to 3-4 inches. Excellent chemical resistance. Enhanced thermal cycling capabilities. Good flow. Serviceable from -100°F to +400°F. Impervious to intermittent exposures to steam. Shore D hardnes >80. |
![]() |
EP42HT-4AOMed Black Thermally conductive, electrically insulative two part epoxy. Meets USP Class VI and ISO 10993-5 certifications. Cryogenically serviceable from 4K to +400F. NASA low outgassing aproved. Black in color. For bonding, sealing, coating and casting. |
![]() |
EP45AOHT Thermally conductive/eletrically insulative epoxy serviceable from -60°F to +500°F. Heat curing. Paste viscosity. Superior chemical resistance properties. Gap filling. Long pot life. Withstands thermal cycling. Gray color. |
![]() |
EP45HTAN Thermally conductive/eletrically insulative epoxy serviceable from 4K to +500°F. Heat curing. Excellent strength retention at high temperatures. High dimensional stability and low shrinkage upon cure. Superior chemical resistance properties. |
![]() |
EP45HTN Electrically conductive heat resistant epoxy compound. Volume resistivity 5-10 ohm-cm. Service operating temperature range from -80°F to +500°F. Paste viscosity. High tensile and compressive strength properties. Cures at elevated temperatures. 100% reactive. Long pot life. |
![]() |
EP45HTND-2 Non-drip epoxy adhesive resists elevated temperature. Paste consistency. Heat curable. Will not flow when curing. Serviceable from -80°F to +500°F. Withstands aggressive chemical exposure. Gap filling. High tensile lap shear and tensile modulus strength. Top notch electrical insulator. |
![]() |
EP45HTQ Quartz filled heat resistant epoxy system. Two component structural adhesive. Durable. High compressive strength. Requires elevated temperature cure. Long pot life. Can be applied on vertical surfaces without dripping. Serviceable from -60°F to +500°F. |
![]() |
EP46HT-1AO Thermally conductive/electrically insulative heat resistant epoxy compound. Requires oven curing. Meets NASA low outgassing specifications. Meets MIL-STD-883J Section 3.5.2 for thermal stability. Excellent dimensional stability. Withstands 1,000 hours 85°C/85% RH. Serviceable from -100°F to +550°F. Tg 215-220°C. |