UV15DC80-FHC UV15DC80-FHC

UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator.

UV15DC80LV One Part UV Curable Epoxy UV15DC80LV

UV and/or heat curable modified epoxy resin system. One component 100% reactive adhesive, sealant, coating. Thermal cure at 80°C for 40-60 minutes. High bond strength. Resists moisture and chemical exposure. Serviceable up to 350°F.

UV15DC80LV-FHC One Part Dual Curing Adhesive UV15DC80LV-FHC

UV and/or heat curable modified epoxy resin system. One component 100% reactive adhesive, sealant, coating. Thermal cure at 80°C for 40-60 minutes. High bond strength. Resists moisture and chemical exposure. Serviceable up to 350°F.

UV15DC80Med One Part UV & Heat Curing Epoxy UV15DC80Med

USP Class VI approved one component UV and heat curable epoxy. Passes ISO 10993-5 cytotoxicity testing. Cures at temperatures as low as 80°C. Moderate viscosity. Minimal shrinkage upon cure. Capable of withstanding liquid sterilants, radiation, autoclaving. Serviceable from -60°F to +400°F.

UV15DC80ND One Part UV System UV15DC80ND

UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator.

UV15DC80TK One Part UV and Heat Curable Epoxy UV15DC80TK

UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Passes 1,000 hours at 85°C/85% humidity. Convenient no mix system. Serviceable from -60°F to +350°F. Superb electrical insulator.

UV15FL One Part UV Curable Epoxy UV15FL

Low viscosity epoxy system with enhanced toughness. Substantial temperature resistance, especially when post cured with heat. 100% reactive. Shore D hardnes >75. Tensile strength >5,000 psi. Optically clear, spin coatable. Serviceable from -80°F to +350°F.

UV15LV One Part UV Curable Epoxy Based Compound UV15LV

Low viscosity, high strength epoxy resin based formulation. Enhanced thermal stability. Cationic curing system. Excellent light transmission properties. Superb electrical insulation characteristics. Serviceable from -80°F to +300°F.

Red colored UV curable epoxy system UV15RCL

Red colored UV curable epoxy system turns clear upon exposure to UV light. Low viscosity, with superb thermal stability. Also capable of spin coating. Outstanding optical clarity. High bond strength. Serviceable from -80°F to +350°F.

UV15TK One Part UV Curable System UV15TK

Moderate viscosity single part UV curable epoxy. Cures quickly. Excellent dimensional stability. Enhanced temperature resistance. Cationic curing system. Optically clear. Volume resistivit >1014. Serviceable from -80°F to +400°F.