EP34CA Two Part Epoxy EP34CA

Resists -80°F to +500°F. Two component epoxy system. Long open time. Good flow properties. Can cure in section exceeding 1/4 inch thick. Withstands 1,000 hours 85°C/85% RH. Protects against aggressive chemical exposure.

EP34LV Two Part Epoxy EP34LV

Two part moderate viscosity epoxy adhesive, sealant, coating. Features high temperature resistance. Superb electrical insulation properties. Service temperature range -60°F to +450°F. Excellent bond strength. Easily machinable. Successfully tested for 1,000 hours 85°C/85% RH.

EP35 Two Part Epoxy EP35

High viscosity epoxy adhesive offers excellent thermal stability. Serviceable from -60°F to +450-500°F. Durable. High strength bonds are maintained even after long-term exposures to elevated temperatures. Outstanding resistance to chemical exposure.

EP35AOLV

Thermally conductive, electrically isolating epoxy serviceable from -60°F to +500°F. Heat curing, good flow. Superior chemical resistance properties. Long pot life. High compressive strength and dimensionally stable.

EP35SP Two Part Epoxy EP35SP

High temperature resistant epoxy system. Withstands exposure to aggressive chemicals. Paste viscosity. 100 to 50 mix ratio by weight. Service temperature range -80°F to +550°F. Excellent compatibility with filament winding and bonding composites.

EP35SP Type V Two Part Epoxy EP35SP Type V

Tough, high temperature resistant heat curing epoxy adhesive. Service temperature range from -80°F to +500°F. Durable, high strength bonds even after prolonged exposure to high temperatures. Ability to withstand thermal cycling and chemical exposure.

EP35TDC Two Part Epoxy EP35TDC

Tough, room temperature curing epoxy paste adhesive for high temperature bonding. Serviceable from -60°F to +450-500°F. Non-drip system. Gap filling. Resistant against thermal cycling and chemical exposure.

EP36 One Part B-Stage Epoxy EP36

One part B-staged epoxy. Flexibilized and toughened. Withstands rigorous thermal cycling and thermal shocks. Superb electrical insulation properties. Ideal for potting/encapsulation. Serviceable from -100°F to +500°F. Available in 30 gram cookies.

EP36AN One Component, B-stage Epoxy EP36AN

Thermally conductive/electrically insulative B-stage epoxy potting/bonding compound. Outstanding toughness and flexibility. Resists up to 500°F. Ability to withstand thermal cycling and impact/vibration. Shore D hardness 80. Volume resistivity 1014 ohm-cm.

EP36AO One Component B-stage Epoxy EP36AO

Thermally conductive, electrically insulative B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies. Meets NASA low outgassing specifications.