Supreme 3HT-80 One Component Epoxy System Supreme 3HT-80

Fast cures at ambient 175°F (80°C). Recommended for bonding heat sensitive substrates. Outstanding thermal cycling capabilities. Single part no mix system. Serviceable from -100°F to +350°F. Tough and durable. Withstands 1,000 hours at 85°C/85% RH.

Supreme 3HTLV One Part Epoxy Adhesive System Supreme 3HTLV

One part, lower viscosity, oven curing epoxy system with very good adhesion to a wide range of plastics. Especially well suited for bonding dissimilar plastic materials. Resists -100°F to +350°F. Exceptional toughness.

Supreme 3HTND-1SM One Part Epoxy System Supreme 3HTND-1SM

One part, oven curing system (cures at 125-150°C) with rapid curing. Good physical properties. Paste consistency. Recommended for surface mounting. Void filling. Low ioinic impurities. Superior "green" strength. No stringing. Withstands thermal stress. Consistent dot profile. Can be automatically dispensed for high volume applications. Serviceable from -100°F to +350°F.

Supreme 3HTND-2CCM One Part Epoxy Supreme 3HTND-2CCM

Toughened epoxy system for bonding, sealing, coating, encapsulation, glob topping. Requires no mixing. Rapid heat curing Passes NASA low outgassing testing. Transfers heat efficiently. Ideal rheology and flow for multiple applications. Stellar electrical insulation properties. Serviceable from -100°F to +400°F.

Supreme 3HTND-2DA One Part Epoxy Supreme 3HTND-2DA

One component, fast curing die attach adhesive. Excellent die shear strength. Serviceable from -100°F to +400°F. Low ionics. Superior thermal conductivity and electrical insulation properties. Dispenses smoothly without tailing or bleed out. Cures in 5-10 minutes at 150°C. NASA low outgassing approved. Available in syringes. Well suited for automatic dispensing. Performed well in 85°C/85% RH testing.

Supreme 3HTND-2DM One Component Epoxy Supreme 3HTND-2DM

Toughened epoxy paste system for damming applications. Requires no mixing. Rapid heat curing. Passes NASA low outgassing testing. Transfers heat efficiently. Stellar electrical insulation properties. Serviceable from -100°F to +400°F.

One Part Epoxy Supreme 3HTND-2DM-1 Supreme 3HTND-2DM-1

Toughened epoxy system for bonding, sealing and specialty dam-and-fill encapsulation. Requires no mixing. Rapid heat curing. Passes NASA low outgassing testing. Transfers heat efficiently. Stellar electrical insulation properties. Serviceable from -100°F to +400°F.

Supreme 3HTND-2GT One Part Epoxy System Supreme 3HTND-2GT

Superior one part glob top. Outstanding dimensional stability and temperature resistance. Fast cures at 125-150°C. Ideal flow for glob topping. Serviceable from -100°F to +400°F. Excellent electrical insulation properties. Low shrinkage. Resists thermal cycling.

One component, silver conductive epoxy adhesive featuring high bond strength Supreme 3HTS-80

One component, silver conductive epoxy adhesive featuring high shear and high peel strengths. Cures at 175°F to 185°F. Bonds well to many substrates. Single part no mix system. Serviceable from -100°F to +350°F. Requires refrigeration, no freezing necessary

Supreme 42HT-2 Two Part Epoxy Supreme 42HT-2

High temperature resistant epoxy adhesive. Toughened. Excellent bond strength. Withstands exposure to many acids, bases, solvents, fuels and oils. Easy application. Service temperature range -80°F to +450°F. Good flow properties. Low exotherm. Long working life. Reliable electrical insulator. Resists thermal cycling.