Supreme 33CLV Two Part Epoxy
Supreme 33CLV
Toughened, two component epoxy for bonding, sealing and coating
Tensile Lap Shear Strength
2,200-2,400 psi
Tensile Modulus
300,000-350,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
  • Encapsulation
Part A: 40,000-70,000 cps, Part B: 2,500-5,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours 75-80 Shore D -100°F to +425°F /tds/supreme-33clv
Supreme 33ND Two Part Epoxy System
Supreme 33ND
Two component, toughened epoxy for bonding and sealing with high temperature resistance
Coefficient of Thermal Expansion
35-40 x 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
115-120°C
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: paste 75°F: 48-72 hours; 200°F: 2-3 hours 75-85 Shore D 4K to +425°F /tds/supreme-33nd
Supreme 34CA Two Component Epoxy
Supreme 34CA
Two component epoxy system for bonding, sealing and coating applications
Tensile Lap Shear Strength
>2,500 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
7,000-20,000 cps gel for 1 hour at 110°C followed by 2-3 hours at 125-150°C >75 Shore D -80°F to +500°F /tds/supreme-34ca
Supreme 3CCM-85 One Component Epoxy Compound
Supreme 3CCM-85
One component, toughened epoxy system for bonding, sealing, coating and encapsulating
Tensile Strength
2,000-3,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
35,000-95,000 cps Cures at 175-185°F for 2 to 3 hours 75-85 Shore D -100°F to +350°F /tds/supreme-3ccm-85
Supreme 3DM-85 One Component Epoxy
Supreme 3DM-85
One component, toughened epoxy system for bonding, sealing, and dam-and-fill encapsulation
Tensile Strength
2,000-3,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
35,000-95,000 cps Cures at 185°F for 2 to 3 hours 75-85 Shore D -100°F to +350°F /tds/supreme-3dm-85
Supreme 3HT One Part Epoxy System
Supreme 3HT
One component, toughened epoxy adhesive, sealant and coating
Dielectric Constant
3.9
Tensile Lap Shear Strength
1,600-1,800 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
100,000-200,000 cps 250°F for 20-30 minutes, 300°F for 5-10 minutes 80-90 Shore D -100°F to +350°F /tds/supreme-3ht
Supreme 3HTND-2CCM One Part Epoxy
Supreme 3HTND-2CCM
One component, toughened epoxy system for bonding, sealing, coating and encapsulating
Glass Transition Temperature (Tg)
90°C
Tensile Modulus
250,000-300,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
paste 250°F for 20-30 minutes or 300°F for 5-10 minutes 80-90 Shore D -100°F to +400°F /tds/supreme-3htnd-2ccm
Supreme 3HTND-2DA One Part Epoxy
Supreme 3HTND-2DA
One component, toughened, electrically insulating epoxy for die attach applications
Coefficient of Thermal Expansion
25-30 X 10⁻⁶ in/in/°C
Dielectric Constant
4.5
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Die Attach
>300,000 cps 5-10 minutes at 150°C >70 Shore D -100°F to +400°F /tds/supreme-3htnd-2da
One Part Epoxy Supreme 3HTND-2DM-1
Supreme 3HTND-2DM-1
One component epoxy featuring non drip consistency for bonding, sealing and specialty dam-and-fill encapsulation
Dielectric Constant
4.6 @ 75°F, 60 Hz
Tensile Modulus
300,000-350,000 psi
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
paste 20-30 minutes at 250°F or 5-10 minutes at 300°F 80-90 Shore D -100°F to +400°F /tds/supreme-3htnd-2dm-1
One component, silver conductive epoxy adhesive featuring high bond strength
Supreme 3HTS-80
One component, toughened, silver conductive epoxy system
Tensile Lap Shear Strength
400-500 psi
Volume Resistivity
<0.05 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste Cures at 175°F to 185°F for 2 to 3 hours 50-60 Shore D -100°F to +350°F /tds/supreme-3hts-80