One Component, No Mix, Toughened Epoxy for Bonding, Sealing and Coating Featuring Very Fast Curing, High Shear and Peel Strength Properties along with Superior Thermal Cycling Capabilities.
Two Component Nickel Conductive Epoxy Adhesive for High Performance Bonding Featuring High Peel Strength, Superior Toughness and Low Volume Resistivity
Room Temperature Curing, Toughened Two Component Epoxy Adhesive for General Purpose Bonding and Sealing; Features High Peel Strength and Shock Resistance.
Two Component, Heat Resistant, Epoxy System for High Performance Bonding, Sealing and Casting. Features a Glass Transition Temperature in Excess of 220°C; Requires Elevated Temperature Curing at 250°F or Above.
Two Component, High Temperature Resistant Epoxy System for High Performance Bonding, Sealing and Coating Featuring Superior Thermal Cycling Capabilities.