MasterSil 150 Two Part Silicone MasterSil 150

Two component, low viscosity condensation cured system. Used for potting and encapsulation. Superior toughness and resiliency. Protects against dust, moisture, ozone, thermal shock and vibration. Excellent thermal stability. Serviceable from -55°F to +400°F.

MasterSil 151 Two Part Silicone System MasterSil 151

Optically clear, addition curing potting, encapsulation, sealing compound. Low shrinkage upon cure. Resists up to +400°F [+204°C]. Shore A hardness 50-60. Highly resistant to water. Long pot life.

MasterSil 151AO Two Part Silicone System MasterSil 151AO

Thermally conductive silicone casting, potting and sealing system. Thermal conductivity of 0.35-.0.54 W/(m•K). Electrically isolating. Low viscosity system bonds well to a wide variety of substrates. Remarkable flexibility. Temperature resistant from -65°F to +400°F. White color.

MasterSil 151Med Two Part Silicone MasterSil 151Med

Medical grade, USP Class VI approved silicone. Addition type cure system. Optically clear. Low outgassing. Offers ambient or elevated temperature cures. Excellent for potting and encapsulation applications. Low shrinkage upon cure. Resists gamma radiation, EtO and various chemical sterilants. Serviceable from -65°F to +400°F.

MasterSil 151S Two Part Silicone System MasterSil 151S

Addition curing, two part silicone for use as an adhesive, sealant, coating or form-in-place gasketing material. Despite its silicone chemistry, it passes NASA low outgassing specifications. It is ideal for applications where low stress is required.

MasterSil 151TC Two Part Silicone MasterSil 151TC

Optically clear, addition curing potting, encapsulation, sealing compound. Low shrinkage upon cure. Resists up to +400°F [+204°C]. Shore A hardness 50-60. Highly resistant to water. Long pot life. Primarily in thermal management applications.

MasterSil 152 Two Part Silicone System MasterSil 152

Low viscosity, optically clear condensation curing system. Superb flexibility and electrical insulation properties. Long pot life. Will cure in section >1 inch. Low exotherm. Elongation 150-180%. Serviceable from -65°F to +400°F.

MasterSil 153 Two Part Silicone MasterSil 153

Two part silicone paste for bonding and sealing applications. Outstanding flexibility. Low exotherm and long pot life system. Self priming feature. Contains no solvents or diluents. Superior electrical insulation properties. Can cure in wide sections vertically and horizontally. Serviceable from -65°F to +400°F

MasterSil 153AO Two Part Silicone System MasterSil 153AO

Thermally conductive silicone casting, potting and sealing system. Thermal conductivity of 0.35-.0.54 W/(m•K). Electrically isolating. Low viscosity system bonds well to a wide variety of substrates. Remarkable flexibility. Temperature resistant from -65°F to +400°F. White color.

MasterSil 153Med Two Part Silicone MasterSil 153Med

Paste consistency. Convenient one to one mix ratio. Elongation 400-500%. Highly water resistant. Self priming feature. Meets USP Class VI and ISO 10993-5 requirements. Superior thermal stability. Resists vibration, shock. Serviceable from -65°F to +400°F.