442 products match
|
EP62-1 Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. |
|
EP62-1BF Cures rapidly at moderate elevated temperatures. Superior resistance to harsh chemicals. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +500°F. Tg 170-175°C. Shore D hardness 80-90. |
|
EP62-1HT Superior resistance to harsh chemicals, particularly to acids. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-160°C. Shore D hardness 80-90. |
|
EP62-1HTMed Black Superior sterilization resistance. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-155°C. Shore D hardness 80-90. |
|
EP62-1HTMed Superior sterilization resistance. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Ideal for bonding and coating. Good flow. Reliable electrical insulator. Serviceable from -60°F to +450°F. Tg 150-155°C. Shore D hardness 80-90. |
|
EP62-1LO Long working life. Cures quickly at moderate temperatures. Passes NASA low outgassing requirements. T >170°C. Resists exposure to acids, bases, many solvents and other chemicals. Superior bond strength properties. Service operating temperature range from -60°F to +450°F. |
|
EP62-1LPSP Low viscosity, optically clear epoxy with superior electrical insulation properties. Thermal stability. Exceptional chemical resistance. Long working life. Low exotherm. Withstands 1,000 hours 85°C/85% RH. Meets NASA low outgassing specifications. Serviceable from 4K to +400°F. |
|
EP62-1LPSPMed Ultra low viscosity, toughened epoxy with superior electrical insulation properties. Thermal stability. Exceptional sterilization resistance. Long working life. Low exotherm. Passes USP Class VI and ISO 10993-5 requirements. Serviceable from -150°F to +400°F. |
|
EP62-1LPSPMed White Sterilization resistant, cryogenic ISO 10993-5 epoxy for medical device assembly. White pigment. Low viscosity. |
|
EP62-1Med Two part epoxy requiring moderate heat curing (80-120°C). Meets USP Class VI biocompatibility specifications. Superb resistance to repeated autoclaving along with excellent adhesion to high temperature plastics such as Ultem, PEEK, etc. Exceptionally long working life. Outstanding electrical insulation properties. Serviceable from -60°F to +450°F. |