442 products match
|
MasterSil 157 Two component low viscosity silicone system. Ideal for potting and encapsulation. Does not require air for curing. Low exotherm; very long pot life. Enhanced low temperature serviceability. Service temperature range of -175°F to +500°F. Superior electrical insulator. |
|
MasterSil 170 Gel Two part, low viscosity silicone gel for sealing, potting and encapsulating applications. Outstanding flexibility. Superior electrical insulation properties. Exceptional optical clarity. Serviceable from -67°F to +392°F. |
|
MasterSil 323 Two part silicone paste for bonding, sealing and encapsulating applications. Optically clear in thin sections. Outstanding flexibility. Contains no solvents or diluents. Low to moderate viscosity. Low dielectric constant. Addition cured, no by-products released during cure. Serviceable from -65°F to +400°F. |
|
MasterSil 323AO-LO Thermally conductive silicone casting, potting and sealing system. Flowable, meets NASA low outgassing specifications. Electrically isolating. Low viscosity system bonds well to a wide variety of substrates. Flexible. Temperature resistant from -65°F to +400°F. White color. |
|
MasterSil 323Med Black Two part silicone paste for bonding, sealing and encapsulating applications. Opaque in thin sections. Outstanding flexibility. Contains no solvents or diluents. Low to moderate viscosity. Low dielectric constant. Addition cured, no by-products released during cure. Serviceable from -65°F to +400°F. |
|
MasterSil 323Med Two part silicone paste for bonding, sealing and encapsulating applications. Optically clear in thin sections. Outstanding flexibility. Contains no solvents or diluents. Low to moderate viscosity. Low dielectric constant. Addition cured, no by-products released during cure. Serviceable from -65°F to +400°F. |
|
MasterSil 410 Non-sag acetoxy type silicone. Provides protection against vibration and shock. Superb weatherability. Elongation 600%. Serviceable from -75°F to 400°F. |
|
MasterSil 415 Optically clear, room temperature curing, no mix acetoxy type system. Good bond strength and outstanding elasticity. Serviceable from -185°F to 400°F. |
|
MasterSil 702 Non-corrosive, high performance elastomeric adhesive/sealant. Heat resistant up to 450°F. Superior physical strength properties. Electrically insulative. |
|
MasterSil 705 Translucent flowable paste for bonding, sealing, coating, formed-in-place gaskets. Cures upon exposure to atmospheric moisture. Serviceable from -75°F to 400°F. Available in tubes, cartridges. |