UV10TK40

One component, high viscosity UV curable system. Outstanding optical clarity. Tg 140°C. Enhanced chemical resistance. Superb physical strength properties. Reliable electrical insulator. Withstands 1,000 hours 85°C/85% RH. Serviceable from -60°F to +450°F.

One component, high viscosity UV curable system UV10TK40M UV10TK40M

One component, high viscosity UV curable system. Outstanding optical clarity. Tg 140°C. Enhanced chemical resistance. Superb physical strength properties. Reliable electrical insulator. Withstands 1,000 hours 85°C/85% RH. Serviceable from -60°F to +450°F.

UV10TKLO-2 One Component UV Curable Compound UV10TKLO-2

Optically clear, easy to apply UV curable system. Meets NASA low outgassing specifications. Superior electrical insulative properties. High physical strength properties and superior chemical resistance. Vacuum compatible. Serviceable from -60°F to +400°F

UV10TKMed One Part UV Curable Compound UV10TKMed

Biocompatible, high viscosity, UV curable compound. Optically clear. Glass transition temperature of more than 140°C. Rapid curing, no mix system. Withstands repeated sterilization. Meets USP Class VI and ISO 10993-5 cytotoxicity testing requirements. Serviceable from -60°F to +450°F.

UV11-3 UV Curable Coating UV11-3

Extra-hard, super abrasion resistant, optically clear coating. 100% solid system. Superior adhesion to polycarbonates, polymethylmethacrylates and polyvinylchlorides. Viscosity 60 cps at 75°F. High resistance to staining and many common chemicals.

UV15 One Part UV Curable Compound UV15

Low viscosity, rigid UV curable system with superb thermal stability. Also capable of spin coating. Outstanding optical clarity. High bond strength. Serviceable from -80°F to +350°F.

UV15 One Part UV Curable Compound UV15

Low viscosity, rigid UV curable system with superb thermal stability. Also capable of spin coating. Outstanding optical clarity. High bond strength. Serviceable from -80°F to +350°F.

UV15-42C One Part UV System UV15-42C

Single component, UV curable. Unsurpassed dimensional stability. Extended service capability of -65°F to +300°F. High optical clarity. Shore D hardnes >60. Resistant to water, oils, cleaning agents, acids and bases. Excellent toughness.

UV15-7DCNV One Part UV System UV15-7DCNV

Dual cure UV system with a secondary heat cure mechanism (250°F) for “shadowed out” areas (those not available to the UV light source). Optically clear and non-yellowing. Produces tough, durable bonds. Serviceable from -80°F to +300°F.

UV15-7LRI One Part UV System UV15-7LRI

One part, UV curable polymer system. Superior light transmission properties. Low refractive index of 1.481. Excellent dimensional stability. Rapid cure speed. Rigid. Serviceable from -60°F to +250°F.