LED401 White Product Information

LED401 White One Part LED Curing System

One Component, High Viscosity LED Curable System for Bonding, Sealing, Coating and Encapsulation, Cures Completely at 405 nm Wavelength up to 1/8 Inch Thick; Cures Tack-Free Without Any Oxygen Inhibition; Excellent Physical Properties; White Color, Opaque System.

EP62-1LO Product Information

EP62-1LO Two Part Epoxy

Two Component Epoxy Resin System Features a Very Long Pot Life at Ambient Temperatures Combined with Rapid Cures at Moderately Elevated Temperatures and Chemical and High Temperature Resistance. Passes NASA Low Outgassing Tests.

Super Gel 9 Product Information

Super Gel 9 Two Part Urethane Modified Epoxy

Room Temperature Curing, Urethane Modified Epoxy Gel-Like System for Sealing and Encapsulation Cures To a Low Shore A Hardness Ideal for Retrievability

EP33CLV Product Information

EP33CLV Two Part Epoxy

Two Component, Room Temperature Curing Epoxy Adhesive for Bonding, Sealing, Coating and Encapsulation Featuring High Temperature Resistance, Good Dimensional Stability and Excellent Chemical Resistance.

UV25 Product Information

UV25 One Part UV Curable System

One Component, Moderate Viscosity UV Curable System for High Performance Bonding, Sealing, Coating and Casting Featuring Excellent Physical Properties and Dimensional Stability with a Remarkably High Glass Transition Temperature Greater Than 180°C.

EP30HT-LO Product Information

EP30HT-LO Two Part Epoxy System

Two Component, Room Temperature Curing Epoxy for High Performance Bonding, Sealing, Coating and Potting Featuring Optical Clarity and High Temperature Resistance. Meets NASA Low Outgassing Specification ASTM E595.

LED403Med Product Information

LED403Med One Part LED Curing System

One Component, High Viscosity LED Curable System for High Performance Bonding, Sealing, Coating and Encapsulation, Cures Tack-Free Without Any Oxygen Inhibition. Meets USP Class VI Specifications; Also Passes ISO 10993-5 Cytotoxicity Test.

Supreme 10HTND-3 Product Information

Supreme 10HTND-3 One Part Epoxy

One Component, Toughened Epoxy Adhesive/Sealant Featuring Exceptionally High Peel and Shear Strength, Convenient Processing and Serviceability at Cryogenic and High Temperatures. Thoroughly Non-Drip Formulation.

EP21LV-LO Product Information

EP21LV-LO Two Part Epoxy

Two Component, Lower Viscosity, Room Temperature Curing Epoxy System for High Performance Bonding, Sealing, Coating and Encapsulation with Outstanding Physical Properties and Easy Processing. Qualified to NASA Low Outgassing Specifications.

EP30M4LV Product Information

EP30M4LV Two Part Epoxy System

Two Component, Room Temperature Curing, Low Viscosity Epoxy Compound for High Performance Bonding, Sealing, Casting and Potting Offering Superior Chemical Resistance and Excellent Physical Strength Properties.