Supreme 10 One component structural adhesive serviceable up to +350°F. High shear and peel strength. Superior resistance to impact, vibration, thermal cycling, stress fatigue cracking, creep. Gray color. Flowable paste viscosity. |
|
Supreme 10HT One part structural epoxy with high bond strength and excellent adhesion to similar and dissimilar substrates, especially composite materials. Requires oven curing at 250-300°F. NASA low outgassing approved. Serviceable from 4k to +400°F. Tough and durable. 85°C/85% RH resistance. |
|
Supreme 10HTCL Single component toughened epoxy adhesive with good flow properties. Resistant to thermal cycling, mechanical vibration/shock. Tensile lap shear strength 2,800-3,000 psi. T-peel strength 25-30 pli. Cures in 60-75 minutes at 250°F, shorter times at higher temperatures. Successfully tested at 1,000 hours 85°C/85% RH. Serviceable from 4k to +400°F. |
|
Supreme 10HTF-1 Fast curing one component thixotropic paste epoxy. Excellent bond strength. Superb toughness and durability. Viscosity remains constant with time. Solid chemical resistance. Reliable electrical insulator. Serviceable from 4k to +400°F. |
|
Supreme 10HTFL Highly flexible, no mix adhesive. Offers outstanding peel strength. 100% reactive. Superior water and chemical resistance. Successfully tested for 1,000 hours 85°C/85% RH. Withstands rigorous thermal cycling. Serviceable from 4k to +350°F. |
|
Supreme 10HTLV One part structural epoxy with high bond strength and excellent adhesion to similar and dissimilar substrates, especially composite materials. Requires oven curing at 250-300°F. NASA low outgassing approved. Serviceable from 4k to +400°F. Tough and durable. 85°C/85% RH resistance. |
|
|
Supreme 10HTND-3 Toughened, non-drip epoxy adhesive featuring high peel and shear strength properties. 100% reactive. Serviceable from 4k to +400°F. No viscosity change over time. Heat curable. |
|
Supreme 11 High shear/peel strength epoxy adhesive. Two component system offers one to one mix ratio by weight or volume. Temperature range from -100°F to +300°F. Resists impact, thermal shock and stress cracking fatigue. Excellent long-term durability. Easy application. |
|
Supreme 112 Potting, encapsulation, coating, sealing, impregnation compound. Low viscosity, long working life. Superior physical strength. Serviceable from -80°F to 550°F. |
|
Supreme 11HT High peel and shear strength system. Convenient one to one mix ratio. Serviceable from -100°F to +400°F. Superior resistance to impact, thermal shock, vibration and stress fatigue cracking. Excellent toughness. Cures readily at room temperature. User friendly. Dependable dimensional stability. Readily machinable. |