Supreme 42HT-2ND Two Part Epoxy Supreme 42HT-2ND

Non-drip epoxy paste has outstanding temperature and chemical resistance. Superior toughness and thermal cycling capability. Meets low outgassing specifications. Withstands 1,000 hours 85°C/85% RH. Superb electrical insulator. Service temperature range -80°F to +450°F.

Supreme 42HT-2ND-2 Two Component Epoxy Supreme 42HT-2ND-2

Two component, high temperature resistant epoxy adhesive, sealant, coating. Excellent toughness. Paste viscosity . Non-flowing even when heated. Gap filling. Superior thermal cycling capabilities. Chemical resistant. Service temperature range -80°F to +450°F.

Supreme 45HT Two Component Epoxy System Supreme 45HT

Toughened, thermally stable, two component epoxy adhesive, sealant, coating. Excellent peel strength. Superior thermal cycling capabilities. Withstands exposure to acids, bases, solvents, fuels, oils, water. Electrical insulator. Service temperature range -100°F to +450°F.

Master Bond Supreme 45HT-3 Epoxy System Supreme 45HT-3

Toughened, thermally stable, two component epoxy adhesive, sealant, coating. Excellent compressive strength. Abrasion resistant. Withstands exposure to acids, bases, solvents, fuels, oils, water. Electrical insulator. Service temperature range -100°F to +550°F.

Supreme 45HTAO Two Part Epoxy Supreme 45HTAO

Toughened, thermally conductive epoxy compound. Superb electrical insulator. Resists -80°F to +500°F. High strength properties. Two part system. Oven curing. Long-term durability.

Supreme 45HTND Two Part Epoxy Supreme 45HTND

Toughened, non-drip epoxy paste for bonding, sealing, coating. Serviceable from -100°F to +450°F. Two component system has long working life. Heat curing. High peel/shear strength properties. Withstands rigorous thermal cycling.

Supreme 45HTND-2 Two Part Epoxy Supreme 45HTND-2

Paste viscosity. Will not flow when cured. Gap filling. Serviceable from -100°F to +450°F. High peel and shear strength properties. Two part system. Long pot life. Good thermal cycling capabilities. Excellent electrical insulator.

Supreme 45HTND-2LO Black Two Part Epoxy Supreme 45HTND-2LO Black

Toughened, two component, non-drip epoxy paste. Service temperature range -100°F to +450°F. Long working life. Gap filling. Meets NASA low outgassing specifications. Withstands 1,000 hours 85°C/85% RH. Superior electrical insulator. Heat curing.

Supreme 45HTQ Two Part Epoxy Compound Supreme 45HTQ

Two component, toughened, quartz filled epoxy with exceptional abrasion resistance. Heat curing system. Long working life after mixing. High compressive strength. Superb dimensional stability. Serviceable from -60°F to +450°F. Withstands exposure to petrochemicals acids, bases, solvents. Good strength retention at elevated temperatures. Successfully tested for 1,000 at 85°C/85% RH.

Supreme 45HTQ Two Component Epoxy Supreme 45HTQ-4

Toughened, two component silicon carbide filled epoxy. Heat curable. Exceptional abrasion and chemical resistance. Serviceable from -100°F to +450°F. Can withstand high compressive loads and rigorous thermal cycling. Good strength retention at elevated temperatures.