353 products match
EP76M Nickel filled electrically conductive epoxy adhesive. Volume resistivity 5-10 ohm-cm. Cures at ambient temperatures. Convenient one to one mix ratio weight or volume. Serviceable from -60°F to +250°F. High compressive strength. Low shrinkage. Useful for applications requiring shielding and static dissipation. |
|
EP76M-F Fast setting nickel filled electrically conductive epoxy adhesive. Room temperature curing. Volume resistivity 5-10 ohm-cm. Serviceable from -60°F to +250°F. Convenient one to one mix ratio weight or volume. Paste consistency. Good resistance to chemicals. High bond strength. |
|
EP76MHT Two component nickel filled electrically conductive epoxy adhesive. Volume resistivity of 5-10 ohm-cm. Serviceable from -60°F to +400°F. Forgiving one to one mix ratio by weight or volume. High bond strength. Thermal conductivity. Paste like consistency. Superb dimensional stability. Applications include EMI/RFI shielding and static dissipation. |
|
EP77M-1 Silver filled electrically conductive epoxy adhesive. Smooth paste viscosity. Volume resistivit <10-3 ohm-cm. Good rigidity. Formulated to cure at room temperature. Serviceable from -60°F to +300°F. Superb thermal conductivity. Dimensional stability. Available in premixed and frozen syringes. |
|
EP77M-F Rapid room temperature curing silver filled electrically conductive adhesive. One to one mix ratio by weight or volume. Fixture time within 5-7 minutes even in small volumes. Exceptional low volume resistivity. Low outgassing. Superior bond strength to similar/dissimilar substrates/ Serviceable from -60°F to +250°F. |
|
EP77M-FMed Rapid room temperature curing silver filled electrically conductive adhesive. One to one mix ratio by weight or volume. Fixture time within 5-7 minutes even in small volumes. Exceptional low volume resistivity. Low outgassing. Superior bond strength to similar/dissimilar substrates. Serviceable from -60°F to +250°F. |
|
EP79 Cost effective alternative to silver filled epoxy with a silver coated nickel filler. Excellent conductivity and physical properties. Superior durability and thermal cycling capabilities. Cures readily at room temperature. Convenient one to one mix ratio weight or volume. Superb heat dissipation. Low linear shrinkage upon cure. Withstands 1,000 hours 85°C/85% RH. Serviceable from 4k to +275°F. Available in premixed and frozen syringes. |
|
EP79FL Highly flexible, silver coated/nickel filled epoxy system. T-pee >20 pli. Low volume resistivity. High bond strength to similar and dissimilar substrates. Resists exposure to thermal cycling. Serviceable from 4k to +275°F. One to one mix ratio by weight. Ambient temperature curing. 100% reactive. Withstands moisture, chemical exposure. Available in premixed and frozen syringes. |
|
EP88FL Low viscosity, optically clear adhesive. Resistant to thermal cycling and thermal shock. Highly desirable Shore D hardness range. Bonds well to dissimilar substrates. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume. |
|
EP90FR-H Two component high strength flame retardant epoxy system. Meets stringent horizontal burn test portion of the FAR standard 14 CFR 25.853(a). Non-halogenated System. Forgiving one to one mix ratio by weight. Good electrical insulation. Serviceable from -60°F to +250°F. Low shrinkage. |