Supreme 62-1 Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. Excellent toughness. |
![]() |
Supreme 65HT-6 Fast room temperature curing heat resistant epoxy adhesive. Serviceable from -80°F to +400°F. Sets up in 5-10 minutes at room temperatures. High tensile lap shear strength. Superior dimensional stability. Good chemical resistance. Tough bonds. Ability to withstand impact and thermal cycling. |
![]() |
Supreme 70CN Two component, toughened epoxy system for bonding, sealing, coating and potting derived from natural substances. Low shrinkage upon curing. Exceptional wetting properties. Service temperature range is -100°F to +450°F. |
![]() |
UV10 One component, no mix, UV curable adhesive. High strength bonds and superior chemical resistance properties. Low viscosity. Excellent dimensional stability. Fast curing. Serviceable from -60°F to +300°F. |
![]() |
UV10-FD One component, UV curable adhesive contains a flourescent dye for identification. High strength bonds and superior chemical resistance properties. Low viscosity. Excellent dimensional stability. Fast curing. Serviceable from -60°F to +300°F. |
![]() |
UV10LV Exceptionally low viscosity. Fast curing. Outstanding dimensional stability and electrical insulation properties. Superior optical clarity. Chemical resistant. Ideal for spin coating. Excellent adhesion to surface treated metals, glass, plastics including polycarbonates and acrylics. Serviceable from -60°F to +250°F. |
![]() |
UV10Med USP Class VI approved, optically clear adhesive. Fast curing. Resists many chemicals and sterilants. Electrically insulative. High bond strength to metals, glass, plastics such as polycarbonates, acrylics. Serviceable from -60°F to +250°F. |
![]() |
UV10TK Single component, moderate viscosity UV curable system. Outstanding optical clarity. Enhanced chemical and temperature resistance. Exceptional dimensional stability. Easy application. Serviceable from -60°F to +300°F. |
![]() |
UV10TK One component, high viscosity UV curable system. Outstanding optical clarity. Tg up to 115°C. Enhanced chemical resistance. Superb physical strength properties. Reliable electrical insulator. Withstands 1,000 hours 85°C/85% RH. Serviceable from -60°F to +400°F. |
![]() |
UV10TK40 One component, high viscosity UV curable system. Outstanding optical clarity. Tg 140°C. Enhanced chemical resistance. Superb physical strength properties. Reliable electrical insulator. Withstands 1,000 hours 85°C/85% RH. Serviceable from -60°F to +450°F. |