Two Component, Low Viscosity Room Temperature Curable, Epoxy Adhesive, Sealant, Coating & Casting System Featuring Both Outstanding Chemical Resistance is NASA low outgassing approved.
One component, heat cured epoxy system for bonding, sealing, dam-and-fill applications. Resists temperatures up to +600°F. Thermally conductive, electrically insulating.