New Electrically Conductive, Silver Filled Adhesive/Sealant is USP Class VI Approved

Product: EP3HTSMed

Release Date: 01/12/2012

Developed for rigorous bonding and sealing in demanding manufacturing applications, Master Bond EP3HTSMed epoxy system features a rapid cure schedule and a tensile shear strength exceeding 1,000 psi. It is 100% reactive and fully meets USP Class VI requirements for medical applications.

This silver-filled epoxy adhesive/sealant has remarkable electrical conductivity with a volume resistivity less than 0.001 ohm cm. Serviceable over the wide temperature range of -60°F to 400°F, EP3HTSMed is resistant to severe thermal cycling and many chemicals including water, fuels, oil, and most organic solvents.

EP3HTSMed is a thixotropic paste and has a specific gravity of 2.90 at 77°F. It requires no mixing and needs only contact pressure during a simple heat cure of 20 to 40 minutes at 300°F or 40 to 90 minutes at 250°F. With minimal shrinkage during cure and a Shore D hardness of 60 to 80, EP3HTSMed bonds well to a variety of substrates including metals, glass, vulcanized rubbers, ceramics, and many plastics.

Silver in color, this one component adhesive is packaged in syringes or glass jars. EP3HTSMed has a shelf life of 6 months in a glass jar and a shelf life 3 months when stored in a syringe at room temperature.

For Editorial Use

Click below to download this release in the format of your choice.

News Release Images

Click an image to download a high resolution version in JPEG format.

image/jpeg icon image/jpeg 1.68 MB

LATEST PRODUCT

Offering a unique blend of high performance properties, Master Bond MasterSil 153 is often used in a...

LATEST WHITE PAPER

Selecting the right adhesive is a balancing act as engineers attempt to find products that meet conflicting end-use and...