Optically Clear, Two Component Urethane Modified Epoxy Gel Offers Dimensional Stability

Product: Super Gel 9

Release Date: 02/07/2013

Featuring softness and resilience, Master Bond Super Gel 9 is a urethane modified epoxy gel that can be employed in a variety of applications. Some of the most common include the encapsulation of sensitive electronic parts and sealing optical components. This multifunctional system is also widely used in the aerospace, electronic, optical, electro-optical and other specialty industries.

Super Gel 9 has an exceptionally low Shore A hardness of about 5-10. This softness allows it to be easily repairable making it ideal for retrieving components with a sharp knife or razor blade. It will not shatter during this process. These properties also enable Super Gel 9 to withstand rigorous thermal cycling and thermal/mechanical shock.

This product has a two to one mix ratio by weight or volume, along with a low viscosity and exotherm enabling it to be cast in larger sections up to 2-3 inches thick. Super Gel 9 bonds well to an array of substrates, such as metals, glass, ceramics and many rubbers and plastics. It has a long working life of 7-9 hours depending on the mass that is mixed (the smaller the mass, the longer the working life). It resists many chemicals including water, oils and fuels. The service temperature range is -100°F to +200°F. Super Gel 9 is available in ½ pints, pints, quarts, gallons, 5 gallon container kits and gun dispensers.

For Editorial Use

Click below to download this release in the format of your choice.

News Release Images

Click an image to download a high resolution version in JPEG format.

image/jpeg icon image/jpeg 896 KB

LATEST PRODUCT

Master Bond EP30HV, a two component epoxy, features wide applicability in the electronic, electrical,...

LATEST WHITE PAPER

Potting compounds play a vital role in the assembly and long term protection of delicate electronic components. The...