EP37-3FLFAO Product Description

Two Component, Room Temperature Curing, Thermally Conductive, Electrically Isolating Epoxy For Potting, Bonding, Sealing & Coating Features Flexibility and Low Viscosity.
Meets NASA Low Outgassing Specification.

Master Bond EP37 3FLFAO is a two component system for high performance potting, bonding, sealing and coating formulated to cure at room temperature or more rapidly at elevated temperatures. It has a convenient one to one mix ratio by weight or volume. It has an unusual blend of properties including high thermal conductivity, excellent electrical insulation properties, good physical strength and a high degree of flexibility. This system forms tough bonds that are resistant to shock, impact and thermal cycling as well as chemicals including water, oil and many solvents. EP37 3FLFAO has low viscosity with excellent flow characteristics making it ideal as a thermally conductive potting epoxy. It is cryogenically serviceable over the wide temperature range of 4K to 250°F. Parts A and B are off white in color. Master Bond EP37 3FLFAO is widely used in the electronic, electrical, computer, metalworking, aerospace and chemical industries where electrical insulation and heat transfer are required. The uniqueness of EP37 3FLFAO lies in the fact that this thermally conductive system retains a high level of flexibility while having the desirable physical characteristics inherent in epoxies. EP37-3FLFAO has been certified by NASA as a low outgassing epoxy.

Product Advantages

  • Convenient mixing: easy to use, non-critical one to one mix ratio by weight or volume.
  • Long working life; cures readily at room temperature and can be accelerated by heat.
  • High thermal conductivity with excellent electrical insulation properties.
  • High bond strength to a wide variety of substrates; very good adhesive properties.
  • Low viscosity with excellent flowability; ideal for potting and casting.
  • Outstanding flexibility; resists rigorous thermal cycling, mechanical and thermal shocks.
  • Good overall physical strength properties and chemical resistance.
  • Cryogenically serviceable down to 4K.
  • Passes NASA low outgassing requirements.

LATEST PRODUCT

Offering a unique blend of high performance properties, Master Bond MasterSil 153 is often used in a...

LATEST WHITE PAPER

Selecting the right adhesive is a balancing act as engineers attempt to find products that meet conflicting end-use and...