EP3RRLV Product Description

One Part Epoxy System Featuring Low Viscosity and Excellent Physical Properties for High Performance Potting, Encapsulation and Underfill Applications. Features Rapid Cure at 230-250°F

Master Bond Polymer System EP3RRLV is a one component, low viscosity, toughened epoxy for high performance potting, encapsulation and underfill applications featuring rapid curing at temperatures as low as 230-250°F. This unique formulation offers high mechanical strength properties, good thermal shock and heat resistance, as well as superior protection against water and chemicals including many solvents and cleaning agents. It also has excellent electrical insulation properties. EP3RRLV has a broad service temperature range of -80°F to +300°F. It adheres well to metals, ceramics, glass and most plastics. As a one part system, it requires no mixing and has an unlimited working life at room temperature. EP3RRLV is 100% reactive and does not contain any solvents or volatiles. Its shelf life at 75°F is 3 months and at 40°-50°F is 6 months.

EP3RRLV features versatile curing schedules with a 20-30 minute cure at temperatures as low as 230°-250°F and a 10-15 minute cure at 300°F. The color of EP3RRLV is light yellow; other colors are available upon request. EP3RRLV has excellent flowability and is a superb material for potting, encapsulation and casting. A most remarkable property of the EP3RRLV epoxy is its ability to be cast in thicknesses up to an inch, a highly unusual property for a one component system. The combination of rapid curing, no mixing and flowability makes EP3RRLV a highly effective underfill epoxy. EP3RRLV is widely used for microelectronics assembly and packaging applications, especially where good mechanical properties, convenient handling and fast curing are required. EP3RRLV is now available in syringes for manual or automatic dispensing.

LATEST PRODUCT

Developed for rigorous bonding and sealing in demanding manufacturing applications, Master Bond...

LATEST WHITE PAPER

Through heat dissipation, thermally conductive adhesives and potting compounds play a pivotal role in the protection of...