UV24TKLO Product Description

One Component, Moderate Viscosity, UV-Curable System for Bonding, Sealing and Encapsulation Featuring Superior Chemical Resistance. Meets NASA Low Outgassing Requirements.

Master Bond Polymer System UV24TKLO is a one part UV curable epoxy modified formulation for bonding, sealing and encapsulation. It passes the rigorous requirements for low outgassing as per ASTM E-595. Most noteworthy, it has outstanding resistance to chemicals, as described in part below.

UV24TKLO has excellent clarity and optical transmission properties. The best wavelengths for curing are 320-365mn and the energy requirement is 10-40 milliwatts per cm2. This epoxy system is not oxygen inhibited.

UV24TKLO has superb physical strength and electrical insulation properties. The service temperature range is -60° to 300°F. The UV24TKLO can be cured in thicker sections, up to 1/16th of an inch and can be easily "layered" to higher levels. The low outgassing properties enable this UV to be used in a wide array of optical, electro-optical and vacuum applications that until now have not been possible for UV curable systems. It should be noted that to optimize the outgassing properties, the UV24TKLO should be preheated to approximately 50°C for 15 minutes prior to use and then allowed to cool down to room temperature.

LATEST PRODUCT

Offering a unique blend of high performance properties, Master Bond MasterSil 153 is often used in a...

LATEST WHITE PAPER

Selecting the right adhesive is a balancing act as engineers attempt to find products that meet conflicting end-use and...